The porous ceramics at different sintering temperature was prepared, using SiC powder as the aggregate, eutectic mixture sintering aids and the coal power as the pore-former.
以SiC为骨料,添加低共熔混合物烧结促进剂,煤粉作为造孔剂,在不同的温度下烧成制备多孔陶瓷管。
A porous ceramic support comprising alumina and a certain number of sintering aids was prepared by extrusion.
以Al2 O3为骨料 ,添加一定数量的烧结促进剂 ,通过挤出成型 ,在介于 110 0~140 0℃之间的温度下烧成 。