1.The results show that the casting with good quality can be obtained by removing one ingate and adding cooling waterway into mould.
结果表明,采用去掉一个内浇口,增加模具冷却水道的工艺可获得质量较好的铸型。
2.The crack in investment castings is commonly created around ingate due to easily forming superheating at root of ingate.
铸件内浇道根部易出现过热,裂纹一般产生在靠近内浇道处。
3.SCT sets up rain canopy at the ingate to boost up box inspection environment and efficiency
SCT进闸口建雨棚,提高箱检环境及效率
4.Improvement of Ingate Design for Large Plain Parts in Investment Castings
精密铸件大平面上内浇道设置方法的改进
5.Fig. 3 Relationship between casting mass and ingate sectional thermal modulus
图3铸件质量和内浇口截面处模数关系
6.Application of Arc Ingate in Investment Casting
弧形内浇道在精铸件工艺设计中的应用